2. (10) A cobalt matrix is reinforced with \( 25 \% \) tungsten carbide fibers under isostrain eonditions. A force of \( 175,
2. (10) A cobalt matrix is reinforced with tungsten carbide fibers under isostrain eonditions. A force of is applied in the longitudinal direction. The elastic modulus for the matrix is , the elastic modulus for the tungsten carbide is 635 GPa. Determine the elastic modulus for the composite. B. C. D. E. F. G. H. I. none of the above


We have an Answer from Expert

View Expert Answer

Expert Answer







  

E_composite = V_matrix * E_matrix + V_fibers * E_fibers